首页  |  本刊简介  |  编委会  |  投稿须知  |  订阅与联系  |  微信  |  出版道德声明  |  Ei收录本刊数据  |  封面
载银活性炭活化过硫酸钠降解酸性橙7
摘要点击 2100  全文点击 953  投稿时间:2015-05-19  修订日期:2015-06-23
查看HTML全文 查看全文  查看/发表评论  下载PDF阅读器
中文关键词  颗粒活性炭    活化剂  过硫酸钠  酸性橙7
英文关键词  granular activated carbon  silver  activator  persulfate  acid orange 7
作者单位E-mail
王忠明 苏州科技学院环境科学与工程学院, 苏州 215009 wangzmchn@163.com 
黄天寅 苏州科技学院环境科学与工程学院, 苏州 215009 huangtianyin111@sohu.com 
陈家斌 苏州科技学院环境科学与工程学院, 苏州 215009  
李文卫 中国科学技术大学化学与材料科学学院, 合肥 230026  
张黎明 苏州科技学院环境科学与工程学院, 苏州 215009  
中文摘要
      采用硝酸氧化的颗粒活性炭浸渍制备Ag/GAC活化剂,利用N2吸附、 SEM、 FT-IR及XRD对Ag/GAC进行表征,得出Ag成功负载于颗粒活性炭上,并以Ag/GAC在常温常压下活化过硫酸钠(PS)产生硫酸根自由基(SO4 ·)降解偶氮染料酸性橙7(AO7). 考察了Ag负载量、 PS浓度、 Ag/GAC投加量、 初始pH对AO7降解效果的影响. 结果表明,当Ag负载量为12.7 mg ·g-1n(PS) :n(AO7)为120 :1、 Ag/GAC投加量为1.0 g ·L-1,降解180 min后AO7降解率达95.0%以上. 初始pH对Ag/GAC活化PS降解AO7有较大影响,pH为5.0时降解效果最优. 通过紫外可见光谱、 气相色谱-质谱(GC/MS)对AO7降解过程进行了探讨,在降解过程中AO7的偶氮键和萘环结构均被破坏,并检测出主要降解产物有邻苯二甲酸和乙酰苯.
英文摘要
      Granular activated carbon with silver loaded as activator (Ag/GAC) was prepared using impregnation method. N2 adsorption, scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FT-IR) and X-ray diffraction (XRD) were adopted to characterize the Ag/GAC, showing that silver was successfully loaded on granular activated carbon. The oxidation degradation of acid orange 7 (AO7) by the Ag/GAC activated by persulfate (PS) was investigated at ambient temperature. The influences of factors such as Ag loading, PS or Ag/GAC dosages and initial pH on the degradation of AO7 were evaluated. The results demonstrated that the degradation rate of AO7 could reach more than 95.0% after 180 min when the Ag loading content, PS/AO7 molar ratio, the Ag/GAC dosage were 12.7mg ·g-1, 120 :1, 1.0 g ·L-1, respectively. The initial pH had significant effect on the AO7 degradation, with pH 5.0 as the optimal pH for the degradation of AO7. The possible degradation pathway was proposed for the AO7 degradation by using UV-visible spectroscopy and gas chromatography-mass spectrometry (GC/MS). The azo bond and naphthalene ring in the AO7 were destroyed during the degradation, with phthalic acid and acetophenone as the main degradation products.